PropertyAm 355SAE 301 Stainless Steel (Annealed)Difference
Yield strength1,138 MPa275 MPa-76%
Tensile strength1,379 MPa725 MPa-47%
Elongation10 %60 %+500%
Elastic modulus199,948 MPa193,000 MPa-3%
Shear modulus75,842 MPa74,231 MPa-2%
Poisson ratio0.320.3-6%
Density7,806 kg/m³7,850 kg/m³+1%
Reduction in area20 %70 %+250%

Difference is SAE 301 Stainless Steel (Annealed) relative to Am 355. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Am 355
grade
AM-355
standard
MIL-HDBK-5J
heat treatment
SCT850
SAE 301 Stainless Steel (Annealed)
grade
301
standard
SAE
heat treatment
Annealed

About 300-series stainless steels

Austenitic stainless steels gain corrosion resistance from chromium and nickel and are non-magnetic in the annealed condition. 304 covers most general-purpose work; 316 adds molybdenum for chloride and seawater service. They cannot be hardened by heat treatment and rely on cold work for higher strength.

What else is in Engineering Database

Related comparisons

View each material