Home/Compare/Aluminum Alloy/A201.0 vs A357.0

A201.0 vs A357.0

Property comparison of A201.0 and A357.0, both aluminum alloy.

Aluminum Alloy7 compared properties
PropertyA201.0A357.0Difference
Yield strength344.75 MPa275.8 MPa-20%
Tensile strength413.7 MPa344.75 MPa-17%
Elongation3 %5 %+67%
Elastic modulus71,019 MPa71,708 MPa+1%
Shear modulus27,580 MPa26,891 MPa-3%
Poisson ratio0.330.330%
Density2,796 kg/m³2,685 kg/m³-4%

Difference is A357.0 relative to A201.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

A201.0
grade
A201.0
standard
MIL-HDBK-5J
heat treatment
Cast
A357.0
grade
A357.0
standard
MIL-HDBK-5J
heat treatment
Cast