Aluminum Alloy7 compared properties
Property354.0A201.0Difference
Yield strength248.22 MPa344.75 MPa+39%
Tensile strength324.07 MPa413.7 MPa+28%
Elongation3 %3 %0%
Elastic modulus73,087 MPa71,019 MPa-3%
Shear modulus27,580 MPa27,580 MPa0%
Poisson ratio0.330.330%
Density2,713 kg/m³2,796 kg/m³+3%

Difference is A201.0 relative to 354.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

354.0
grade
354.0
standard
MIL-HDBK-5J
heat treatment
Cast
A201.0
grade
A201.0
standard
MIL-HDBK-5J
heat treatment
Cast