Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Aluminum Alloy/355.0 vs A201.0

355.0 vs A201.0

Property comparison of 355.0 and A201.0, both aluminum alloy.

Aluminum Alloy7 compared properties
Property355.0A201.0Difference
Yield strength138 MPa344.75 MPa+150%
Tensile strength221 MPa413.7 MPa+87%
Elongation2 %3 %+50%
Elastic modulus73,000 MPa71,019 MPa-3%
Shear modulus26,000 MPa27,580 MPa+6%
Poisson ratio0.330.330%
Density2,700 kg/m³2,796 kg/m³+4%

Difference is A201.0 relative to 355.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

355.0
standard
ANSI
heat treatment
Cast (T6)
grade
A201.0
standard
MIL-HDBK-5J
heat treatment
Cast
grade
A201.0

What else is in Engineering Database