355.0 vs A357.0
Property comparison of 355.0 and A357.0, both aluminum alloy.
| Property | 355.0 | A357.0 | Difference |
|---|---|---|---|
| Yield strength | 138 MPa | 275.8 MPa | +100% |
| Tensile strength | 221 MPa | 344.75 MPa | +56% |
| Elongation | 2 % | 5 % | +150% |
| Elastic modulus | 73,000 MPa | 71,708 MPa | -2% |
| Shear modulus | 26,000 MPa | 26,891 MPa | +3% |
| Poisson ratio | 0.33 | 0.33 | 0% |
| Density | 2,700 kg/m³ | 2,685 kg/m³ | -1% |
Difference is A357.0 relative to 355.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
355.0
- standard
- ANSI
- heat treatment
- Cast (T6)
- grade
- —
A357.0
- standard
- MIL-HDBK-5J
- heat treatment
- Cast
- grade
- A357.0
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators