A201.0 vs A356.0
Property comparison of A201.0 and A356.0, both aluminum alloy.
| Property | A201.0 | A356.0 | Difference |
|---|---|---|---|
| Yield strength | 344.75 MPa | 165 MPa | -52% |
| Tensile strength | 413.7 MPa | 234 MPa | -43% |
| Elongation | 3 % | 3.5 % | +17% |
| Elastic modulus | 71,019 MPa | 73,000 MPa | +3% |
| Shear modulus | 27,580 MPa | 26,000 MPa | -6% |
| Poisson ratio | 0.33 | 0.33 | 0% |
| Density | 2,796 kg/m³ | 2,700 kg/m³ | -3% |
Difference is A356.0 relative to A201.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
A201.0
- grade
- A201.0
- standard
- MIL-HDBK-5J
- heat treatment
- Cast
A356.0
- grade
- —
- standard
- ANSI
- heat treatment
- Cast (T6)
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators