Aluminum Alloy12 compared properties
Property355.0A356.0Difference
Yield strength138 MPa165 MPa+20%
Tensile strength221 MPa234 MPa+6%
Elongation2 %3.5 %+75%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Brinell hardness70 HB70 HB0%
Thermal conductivity155 W/m·K155 W/m·K0%
Specific heat900 J/kg·K900 J/kg·K0%
Coefficient of thermal expansion0.000021 1/K0.000021 1/K0%
Melting point549 °C557 °C+1%

Difference is A356.0 relative to 355.0. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

355.0
standard
ANSI
heat treatment
Cast (T6)
A356.0
standard
ANSI
heat treatment
Cast (T6)