Property comparison of 310S High-Temperature Austenitic and 317LMN Austenitic, both stainless steel.

Stainless Steel9 compared properties
Property310S High-Temperature Austenitic317LMN AusteniticDifference
Yield strength245 MPa205 MPa-16%
Tensile strength550 MPa550 MPa0%
Elongation45 %40 %-11%
Elastic modulus196,000 MPa200,000 MPa+2%
Density7,890 kg/m³8,000 kg/m³+1%
Thermal conductivity10.8 W/m·K14 W/m·K+30%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K+1%
Melting point1,402 °C1,443 °C+3%

Difference is 317LMN Austenitic relative to 310S High-Temperature Austenitic. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

310S High-Temperature Austenitic
grade
S31008
standard
ASTM A240
heat treatment
Annealed
317LMN Austenitic
grade
S31726
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.