Property comparison of 254 SMO Super-Austenitic and 317LMN Austenitic, both stainless steel.

Stainless Steel7 compared properties
Property254 SMO Super-Austenitic317LMN AusteniticDifference
Yield strength300 MPa205 MPa-32%
Tensile strength650 MPa550 MPa-15%
Elongation35 %40 %+14%
Elastic modulus200,000 MPa200,000 MPa0%
Density8,000 kg/m³8,000 kg/m³0%
Thermal conductivity13 W/m·K14 W/m·K+8%
Specific heat460 J/kg·K460 J/kg·K0%

Difference is 317LMN Austenitic relative to 254 SMO Super-Austenitic. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

254 SMO Super-Austenitic
grade
S31254
standard
ASTM A240
heat treatment
Annealed
317LMN Austenitic
grade
S31726
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material