Property253 MA High-Temperature Austenitic317LMN AusteniticDifference
Yield strength310 MPa205 MPa-34%
Tensile strength650 MPa550 MPa-15%
Elongation40 %40 %0%
Elastic modulus200,000 MPa200,000 MPa0%
Density7,800 kg/m³8,000 kg/m³+3%
Thermal conductivity15 W/m·K14 W/m·K-7%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000019 1/K0.000016 1/K-16%

Difference is 317LMN Austenitic relative to 253 MA High-Temperature Austenitic. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

253 MA High-Temperature Austenitic
grade
S30815
standard
ASTM A240 / EN 10028
heat treatment
Annealed
317LMN Austenitic
grade
S31726
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material