254 SMO Super-Austenitic vs 310S High-Temperature Austenitic

Property comparison of 254 SMO Super-Austenitic and 310S High-Temperature Austenitic, both stainless steel.

Stainless Steel8 compared properties
Property254 SMO Super-Austenitic310S High-Temperature AusteniticDifference
Yield strength300 MPa245 MPa-18%
Tensile strength650 MPa550 MPa-15%
Elongation35 %45 %+29%
Elastic modulus200,000 MPa196,000 MPa-2%
Density8,000 kg/m³7,890 kg/m³-1%
Brinell hardness250 HB217 HB-13%
Thermal conductivity13 W/m·K10.8 W/m·K-17%
Specific heat460 J/kg·K460 J/kg·K0%

Difference is 310S High-Temperature Austenitic relative to 254 SMO Super-Austenitic. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

254 SMO Super-Austenitic
grade
S31254
standard
ASTM A240
heat treatment
Annealed
310S High-Temperature Austenitic
grade
S31008
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.