Thermal Conductivity: abs to cast_iron_malleable
Thermal conductivity of materials — k-values for metals, alloys, insulation, ceramics, and other materials at reference temperature
| material id | category | density kg m3 (kg/m3) | k W mK (W/mK) | material name | temp ref C (C) |
|---|---|---|---|---|---|
| abs | polymer | 1,050 | 0.17 | ABS | 25 |
| antimony | metal | 6,697 | 24 | Antimony | 25 |
| boron | Pure Metal | 2,500 | 27 | Boron | 27 |
| cadmium | metal | 8,650 | 92.048 | Cadmium | 25 |
| cast_iron_malleable | alloy | 7,150 | 40 | Malleable Cast Iron (ASTM A220) | 25 |