Explore the Engineering Database more efficiently by signing up for free. Sign up free

Babbitt-B23-Grade7-Lead — Tin Alloy

Category
Tin Alloy
Material Id
Babbitt B23 Grade7 Lead
Brinell Hardness (HB)
22.5
Cte per K (1/K)
0.000026
Density Kg M3 (kg/m3)
10,000
Elongation Percent (%)
4
Grade
Grade 7 Lead-Base
Heat Treatment
Chill Cast
Melting Point C (°C)
254
Name
Babbitt Grade 7 (Pb-9.3Sn-15Sb) Lead-Base
Standard
ASTM B23
Tensile Strength MPa (MPa)
72
Yield Strength MPa (MPa)
24

Source: ASTM B23