Babbitt-B23-Grade13-Lead — Tin Alloy
- Category
- Tin Alloy
- Material Id
- Babbitt B23 Grade13 Lead
- Brinell Hardness (HB)
- 19
- Cte per K (1/K)
- 0.000026
- Density Kg M3 (kg/m3)
- 10,200
- Elongation Percent (%)
- 5
- Grade
- Grade 13 Lead-Base
- Heat Treatment
- Chill Cast
- Melting Point C (°C)
- 249
- Name
- Babbitt Grade 13 (Pb-6Sn-10Sb) Lead-Base
- Standard
- ASTM B23
- Tensile Strength MPa (MPa)
- 70
- Yield Strength MPa (MPa)
- 23
Source: ASTM B23