Explore the Engineering Database more efficiently by signing up for free. Sign up free
Leaded-Tin-Bronze-C92900 — Copper Alloy
- Category
- Copper Alloy
- Material Id
- Leaded Tin Bronze C92900
- Cte per K (1/K)
- 0.000018
- Density Kg M3 (kg/m3)
- 8,800
- Elastic Modulus MPa (MPa)
- 120,000
- Elongation Percent (%)
- 20
- Melting Point C (°C)
- 960
- Name
- Leaded Tin Bronze C92900
- Poisson Ratio (dimensionless)
- 0.31
- Shear Modulus MPa (MPa)
- 45,000
- Specific Heat J kgK (J/(kg·K))
- 377
- Standard
- ANSI
- Tensile Strength MPa (MPa)
- 324
- Thermal Conductivity W mK (W/(m·K))
- 52
- Yield Strength MPa (MPa)
- 179
Source: ANSI