Csn-423147 — Copper Alloy
- Category
- Copper Alloy
- Material Id
- Csn 423147
- Cte per K (1/K)
- 0.000018
- Density Kg M3 (kg/m3)
- 8,700
- Elastic Modulus MPa (MPa)
- 120,000
- Melting Point C (°C)
- 960
- Name
- Csn 423147
- Poisson Ratio (dimensionless)
- 0.32
- Shear Modulus MPa (MPa)
- 45,000
- Specific Heat J kgK (J/(kg·K))
- 385
- Standard
- Csn
- Tensile Strength MPa (MPa)
- 400
- Thermal Conductivity W mK (W/(m·K))
- 75
- Yield Strength MPa (MPa)
- 130