Csn-423311 — Copper Alloy

Category
Copper Alloy
Material Id
Csn 423311
Cte per K (1/K)
0.000018
Density Kg M3 (kg/m3)
8,700
Elastic Modulus MPa (MPa)
100,000
Melting Point C (°C)
960
Name
Csn 423311
Poisson Ratio (dimensionless)
0.34
Shear Modulus MPa (MPa)
37,000
Specific Heat J kgK (J/(kg·K))
385
Standard
Csn
Tensile Strength MPa (MPa)
600
Thermal Conductivity W mK (W/(m·K))
75
Yield Strength MPa (MPa)
350

Source: CSN