Leaded-Tin-Bronze-C92700 — Copper Alloy

Category
Copper Alloy
Material Id
Leaded Tin Bronze C92700
Cte per K (1/K)
0.000018
Density Kg M3 (kg/m3)
8,800
Elastic Modulus MPa (MPa)
120,000
Elongation Percent (%)
20
Melting Point C (°C)
960
Name
Leaded Tin Bronze C92700
Poisson Ratio (dimensionless)
0.31
Shear Modulus MPa (MPa)
45,000
Specific Heat J kgK (J/(kg·K))
377
Standard
ANSI
Tensile Strength MPa (MPa)
290
Thermal Conductivity W mK (W/(m·K))
52
Yield Strength MPa (MPa)
145

Source: ANSI