High-Leaded-Tin-Bronze-C94300 — Copper Alloy

Category
Copper Alloy
Material Id
High Leaded Tin Bronze C94300
Cte per K (1/K)
0.000019
Density Kg M3 (kg/m3)
8,800
Elastic Modulus MPa (MPa)
120,000
Elongation Percent (%)
15
Melting Point C (°C)
925
Name
High Leaded Tin Bronze C94300
Poisson Ratio (dimensionless)
0.31
Shear Modulus MPa (MPa)
45,000
Specific Heat J kgK (J/(kg·K))
377
Standard
ANSI
Tensile Strength MPa (MPa)
186
Thermal Conductivity W mK (W/(m·K))
50
Yield Strength MPa (MPa)
90

Source: ANSI