Explore the Engineering Database more efficiently by signing up for free. Sign up free

High-Leaded-Tin-Bronze-C93400 — Copper Alloy

Category
Copper Alloy
Material Id
High Leaded Tin Bronze C93400
Cte per K (1/K)
0.000019
Density Kg M3 (kg/m3)
8,930
Elastic Modulus MPa (MPa)
120,000
Elongation Percent (%)
20
Melting Point C (°C)
930
Name
High Leaded Tin Bronze C93400
Poisson Ratio (dimensionless)
0.31
Shear Modulus MPa (MPa)
45,000
Specific Heat J kgK (J/(kg·K))
375
Standard
ANSI
Tensile Strength MPa (MPa)
221
Thermal Conductivity W mK (W/(m·K))
47
Yield Strength MPa (MPa)
110

Source: ANSI

copper_alloy — material id High_Leaded_Tin_Bronze_C93400 · name High Leaded Tin Bronze C93400 · tensile strength MPa 221 MPa · yield strength MPa 110 MPa · elongation percent 20 % | Metal Alloy Properties | Engineering Database