Explore the Engineering Database more efficiently by signing up for free. Sign up free
High-Copper-Alloy-C81700 — Copper Alloy
- Category
- Copper Alloy
- Material Id
- High-Copper Alloy C81700
- Cte per K (1/K)
- 0.000017
- Density Kg M3 (kg/m3)
- 8,830
- Elastic Modulus MPa (MPa)
- 108,000
- Elongation Percent (%)
- 8
- Melting Point C (°C)
- 1,060
- Name
- High-Copper Alloy C81700
- Poisson Ratio (dimensionless)
- 0.35
- Shear Modulus MPa (MPa)
- 40,000
- Specific Heat J kgK (J/(kg·K))
- 383
- Standard
- ANSI
- Tensile Strength MPa (MPa)
- 634
- Thermal Conductivity W mK (W/(m·K))
- 315
- Yield Strength MPa (MPa)
- 469
Source: ANSI