70-2014-Forging-T652-5.001-6.000-S — 2014 Forging T652
- Material Id
- 2014 Forging T652 5.001-6.000 S
- Temp F
- 70
- E Msi (Msi)
- 10.5
- Ec Msi (Msi)
- 10.8
- Fbru Ksi (ksi)
- 83
- Fbru Ksi 2 (ksi)
- 108
- Fbry Ksi (ksi)
- 73
- Fbry Ksi 2 (ksi)
- 86
- Fcy Ksi (ksi)
- 53
- Fcy Ksi Lt (ksi)
- 54
- Fcy Ksi St (ksi)
- 55
- Fsu Ksi (ksi)
- 36
- Ftu Ksi (ksi)
- 61
- Ftu Ksi Lt (ksi)
- 61
- Ftu Ksi St (ksi)
- 59
- Fty Ksi (ksi)
- 53
- Fty Ksi Lt (ksi)
- 53
- Fty Ksi St (ksi)
- 50
- G Msi (Msi)
- 4
- Basis
- S
- Condition
- T652b
- Density Lb IN3 (lb/in^3)
- 0.101
- Elongation Pct (%)
- 7
- Elongation Pct Lt (%)
- 2
- Elongation Pct St (%)
- 1
- Form
- Hand Forging
- Poisson Ratio
- 0.33
- Specification
- AMS-a-22771 and AMS-Qq-a-367
- Thickness Range
- 5.001-6.000