Zinc Alloy10 compared properties
PropertyZA-12 (Zn-11Al-1Cu-0.02Mg)Zamak 7 (Zn-4Al-0.4Mg low-impurity)Difference
Yield strength317 MPa221 MPa-30%
Tensile strength400 MPa283 MPa-29%
Elongation6 %13 %+117%
Elastic modulus83,000 MPa85,000 MPa+2%
Density6,000 kg/m³6,600 kg/m³+10%
Brinell hardness105 HB80 HB-24%
Thermal conductivity116 W/m·K113 W/m·K-3%
Specific heat448 J/kg·K419 J/kg·K-6%
Coefficient of thermal expansion0.000024 1/K0.000027 1/K+15%
Melting point405 °C384 °C-5%

Difference is Zamak 7 (Zn-4Al-0.4Mg low-impurity) relative to ZA-12 (Zn-11Al-1Cu-0.02Mg). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ZA-12 (Zn-11Al-1Cu-0.02Mg)
standard
ASTM B86
heat treatment
die cast
grade
Zamak 7 (Zn-4Al-0.4Mg low-impurity)
standard
ASTM B86
heat treatment
die cast
grade
AG40B

What else is in Engineering Database

Related comparisons

View each material