Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Zinc Alloy/ZA-8 (Zn-8Al-1Cu-0.02Mg) vs Zamak 7 (Zn-4Al-0.4Mg low-impurity)

ZA-8 (Zn-8Al-1Cu-0.02Mg) vs Zamak 7 (Zn-4Al-0.4Mg low-impurity)

Property comparison of ZA-8 (Zn-8Al-1Cu-0.02Mg) and Zamak 7 (Zn-4Al-0.4Mg low-impurity), both zinc alloy.

Zinc Alloy10 compared properties
PropertyZA-8 (Zn-8Al-1Cu-0.02Mg)Zamak 7 (Zn-4Al-0.4Mg low-impurity)Difference
Yield strength290 MPa221 MPa-24%
Tensile strength374 MPa283 MPa-24%
Elongation8 %13 %+63%
Elastic modulus85,000 MPa85,000 MPa0%
Density6,300 kg/m³6,600 kg/m³+5%
Brinell hardness103 HB80 HB-22%
Thermal conductivity116 W/m·K113 W/m·K-3%
Specific heat448 J/kg·K419 J/kg·K-6%
Coefficient of thermal expansion0.000024 1/K0.000027 1/K+15%
Melting point390 °C384 °C-2%

Difference is Zamak 7 (Zn-4Al-0.4Mg low-impurity) relative to ZA-8 (Zn-8Al-1Cu-0.02Mg). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ZA-8 (Zn-8Al-1Cu-0.02Mg)
standard
ASTM B86
heat treatment
die cast
grade
Zamak 7 (Zn-4Al-0.4Mg low-impurity)
standard
ASTM B86
heat treatment
die cast
grade
AG40B