Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Zinc Alloy/ZA-12 (Zn-11Al-1Cu-0.02Mg) vs ZA-27 (Zn-27Al-2Cu-0.015Mg)

ZA-12 (Zn-11Al-1Cu-0.02Mg) vs ZA-27 (Zn-27Al-2Cu-0.015Mg)

Property comparison of ZA-12 (Zn-11Al-1Cu-0.02Mg) and ZA-27 (Zn-27Al-2Cu-0.015Mg), both zinc alloy.

Zinc Alloy10 compared properties
PropertyZA-12 (Zn-11Al-1Cu-0.02Mg)ZA-27 (Zn-27Al-2Cu-0.015Mg)Difference
Yield strength317 MPa379 MPa+20%
Tensile strength400 MPa421 MPa+5%
Elongation6 %2 %-67%
Elastic modulus83,000 MPa78,000 MPa-6%
Density6,000 kg/m³5,000 kg/m³-17%
Brinell hardness105 HB115 HB+10%
Thermal conductivity116 W/m·K160 W/m·K+38%
Specific heat448 J/kg·K523 J/kg·K+17%
Coefficient of thermal expansion0.000024 1/K0.00002 1/K-16%
Melting point405 °C430 °C+6%

Difference is ZA-27 (Zn-27Al-2Cu-0.015Mg) relative to ZA-12 (Zn-11Al-1Cu-0.02Mg). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ZA-12 (Zn-11Al-1Cu-0.02Mg)
standard
ASTM B86
heat treatment
die cast
ZA-27 (Zn-27Al-2Cu-0.015Mg)
standard
ASTM B86
heat treatment
die cast

What else is in Engineering Database

Related comparisons

View each material