Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Zinc Alloy/ZA-27 (Zn-27Al-2Cu-0.015Mg) vs Zamak 2 (Zn-4Al-3Cu-0.035Mg)

ZA-27 (Zn-27Al-2Cu-0.015Mg) vs Zamak 2 (Zn-4Al-3Cu-0.035Mg)

Property comparison of ZA-27 (Zn-27Al-2Cu-0.015Mg) and Zamak 2 (Zn-4Al-3Cu-0.035Mg), both zinc alloy.

Zinc Alloy10 compared properties
PropertyZA-27 (Zn-27Al-2Cu-0.015Mg)Zamak 2 (Zn-4Al-3Cu-0.035Mg)Difference
Yield strength379 MPa283 MPa-25%
Tensile strength421 MPa359 MPa-15%
Elongation2 %7 %+250%
Elastic modulus78,000 MPa85,000 MPa+9%
Density5,000 kg/m³6,600 kg/m³+32%
Brinell hardness115 HB100 HB-13%
Thermal conductivity160 W/m·K113 W/m·K-29%
Specific heat523 J/kg·K419 J/kg·K-20%
Coefficient of thermal expansion0.00002 1/K0.000027 1/K+37%
Melting point430 °C385 °C-10%

Difference is Zamak 2 (Zn-4Al-3Cu-0.035Mg) relative to ZA-27 (Zn-27Al-2Cu-0.015Mg). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ZA-27 (Zn-27Al-2Cu-0.015Mg)
standard
ASTM B86
heat treatment
die cast
grade
Zamak 2 (Zn-4Al-3Cu-0.035Mg)
standard
ASTM B86
heat treatment
die cast
grade
AC43A