PropertyW-3Re (W-3%Re) annealedZircadyne 702 (UNS R60702)Difference
Yield strength900 MPa321.1 MPa-64%
Tensile strength1,100 MPa468.1 MPa-57%
Elongation8 %28.9 %+261%
Elastic modulus388,000 MPa99,200 MPa-74%
Density19,600 kg/m³6,510 kg/m³-67%
Thermal conductivity100 W/m·K22 W/m·K-78%
Coefficient of thermal expansion0.000005 1/K0.000006 1/K+26%
Melting point3,170 °C1,852 °C-42%

Difference is Zircadyne 702 (UNS R60702) relative to W-3Re (W-3%Re) annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

W-3Re (W-3%Re) annealed
standard
ASM Alloy Digest / PMC review of W-Re alloys (PMC10779616)
heat treatment
annealed
grade
Zircadyne 702 (UNS R60702)
standard
ASTM B551 / B523 / B493 / B550 / B658
heat treatment
Annealed
grade
R60702

What else is in Engineering Database

Related comparisons

View each material