PropertyTungsten (W pure >99.95%)W-3Re (W-3%Re) annealedDifference
Yield strength750 MPa900 MPa+20%
Tensile strength980 MPa1,100 MPa+12%
Elongation2 %8 %+300%
Elastic modulus400,000 MPa388,000 MPa-3%
Density19,300 kg/m³19,600 kg/m³+2%
Thermal conductivity173 W/m·K100 W/m·K-42%
Coefficient of thermal expansion0.000005 1/K0.000005 1/K+2%
Melting point3,422 °C3,170 °C-7%

Difference is W-3Re (W-3%Re) annealed relative to Tungsten (W pure >99.95%). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Tungsten (W pure >99.95%)
grade
W pure
standard
ASTM
heat treatment
Stress-Relieved
W-3Re (W-3%Re) annealed
grade
standard
ASM Alloy Digest / PMC review of W-Re alloys (PMC10779616)
heat treatment
annealed

What else is in Engineering Database

Related comparisons

View each material