PropertyTZM (Mo-0.5Ti-0.08Zr)W-3Re (W-3%Re) annealedDifference
Yield strength860 MPa900 MPa+5%
Tensile strength965 MPa1,100 MPa+14%
Elastic modulus329,000 MPa388,000 MPa+18%
Density10,160 kg/m³19,600 kg/m³+93%
Thermal conductivity54 W/m·K100 W/m·K+85%
Coefficient of thermal expansion0.000005 1/K0.000005 1/K-13%
Melting point2,620 °C3,170 °C+21%

Difference is W-3Re (W-3%Re) annealed relative to TZM (Mo-0.5Ti-0.08Zr). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

TZM (Mo-0.5Ti-0.08Zr)
grade
R03630
standard
Plansee product data / ASTM B386 Grade 364
heat treatment
stress-relieved
W-3Re (W-3%Re) annealed
grade
standard
ASM Alloy Digest / PMC review of W-Re alloys (PMC10779616)
heat treatment
annealed