Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Refractory/Vanadium (V pure >99.7%) vs W-25Re (W-25%Re) annealed

Vanadium (V pure >99.7%) vs W-25Re (W-25%Re) annealed

Property comparison of Vanadium (V pure >99.7%) and W-25Re (W-25%Re) annealed, both refractory.

Refractory4 compared properties
PropertyVanadium (V pure >99.7%)W-25Re (W-25%Re) annealedDifference
Elastic modulus128,000 MPa390,000 MPa+205%
Density6,110 kg/m³19,700 kg/m³+222%
Coefficient of thermal expansion0.000008 1/K0.000005 1/K-39%
Melting point1,910 °C3,050 °C+60%

Difference is W-25Re (W-25%Re) annealed relative to Vanadium (V pure >99.7%). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Vanadium (V pure >99.7%)
grade
R02030
standard
CRC Handbook of Chemistry and Physics 103rd Ed.
heat treatment
annealed
W-25Re (W-25%Re) annealed
grade
standard
ASM Alloy Digest W-25Re (WAH CHANG W-25Re) / multiple supplier datasheets
heat treatment
annealed