Home/Compare/Refractory/TZM (Mo-0.5Ti-0.08Zr) vs W-25Re (W-25%Re) annealed

TZM (Mo-0.5Ti-0.08Zr) vs W-25Re (W-25%Re) annealed

Property comparison of TZM (Mo-0.5Ti-0.08Zr) and W-25Re (W-25%Re) annealed, both refractory.

Refractory5 compared properties
PropertyTZM (Mo-0.5Ti-0.08Zr)W-25Re (W-25%Re) annealedDifference
Tensile strength965 MPa1,650 MPa+71%
Elastic modulus329,000 MPa390,000 MPa+19%
Density10,160 kg/m³19,700 kg/m³+94%
Coefficient of thermal expansion0.000005 1/K0.000005 1/K-4%
Melting point2,620 °C3,050 °C+16%

Difference is W-25Re (W-25%Re) annealed relative to TZM (Mo-0.5Ti-0.08Zr). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

TZM (Mo-0.5Ti-0.08Zr)
grade
R03630
standard
Plansee product data / ASTM B386 Grade 364
heat treatment
stress-relieved
W-25Re (W-25%Re) annealed
grade
standard
ASM Alloy Digest W-25Re (WAH CHANG W-25Re) / multiple supplier datasheets
heat treatment
annealed