Vanadium (V pure >99.7%) vs Zircadyne 702 (UNS R60702)

Property comparison of Vanadium (V pure >99.7%) and Zircadyne 702 (UNS R60702), both refractory.

Refractory8 compared properties
PropertyVanadium (V pure >99.7%)Zircadyne 702 (UNS R60702)Difference
Elastic modulus128,000 MPa99,200 MPa-23%
Shear modulus47,000 MPa36,200 MPa-23%
Poisson ratio0.370.35-5%
Density6,110 kg/m³6,510 kg/m³+7%
Thermal conductivity31 W/m·K22 W/m·K-29%
Specific heat489 J/kg·K284.7 J/kg·K-42%
Coefficient of thermal expansion0.000008 1/K0.000006 1/K-31%
Melting point1,910 °C1,852 °C-3%

Difference is Zircadyne 702 (UNS R60702) relative to Vanadium (V pure >99.7%). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Vanadium (V pure >99.7%)
grade
R02030
standard
CRC Handbook of Chemistry and Physics 103rd Ed.
heat treatment
annealed
Zircadyne 702 (UNS R60702)
grade
R60702
standard
ASTM B551 / B523 / B493 / B550 / B658
heat treatment
Annealed