Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Refractory/Tantalum (Ta pure >99.7%) vs Tungsten (W pure >99.95%)

Tantalum (Ta pure >99.7%) vs Tungsten (W pure >99.95%)

Property comparison of Tantalum (Ta pure >99.7%) and Tungsten (W pure >99.95%), both refractory.

Refractory12 compared properties
PropertyTantalum (Ta pure >99.7%)Tungsten (W pure >99.95%)Difference
Yield strength165 MPa750 MPa+355%
Tensile strength270 MPa980 MPa+263%
Elongation30 %2 %-93%
Elastic modulus186,000 MPa400,000 MPa+115%
Shear modulus68,000 MPa156,000 MPa+129%
Poisson ratio0.350.28-20%
Density16,650 kg/m³19,300 kg/m³+16%
Brinell hardness100 HB310 HB+210%
Thermal conductivity57 W/m·K173 W/m·K+204%
Specific heat140 J/kg·K134 J/kg·K-4%
Coefficient of thermal expansion0.000007 1/K0.000005 1/K-31%
Melting point2,996 °C3,422 °C+14%

Difference is Tungsten (W pure >99.95%) relative to Tantalum (Ta pure >99.7%). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Tantalum (Ta pure >99.7%)
grade
Ta R05200
standard
ASTM
heat treatment
Annealed
Tungsten (W pure >99.95%)
grade
W pure
standard
ASTM
heat treatment
Stress-Relieved

What else is in Engineering Database

Related comparisons

View each material