Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Cobalt Alloy/Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast vs Tribaloy T-800 (Co-28Mo-17Cr-3.4Si) cast

Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast vs Tribaloy T-800 (Co-28Mo-17Cr-3.4Si) cast

Property comparison of Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast and Tribaloy T-800 (Co-28Mo-17Cr-3.4Si) cast, both cobalt alloy.

Cobalt Alloy3 compared properties
PropertyTribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) castTribaloy T-800 (Co-28Mo-17Cr-3.4Si) castDifference
Density8,900 kg/m³8,600 kg/m³-3%
Brinell hardness55 HB58 HB+5%
Melting point1,314 °C1,320 °C0%

Difference is Tribaloy T-800 (Co-28Mo-17Cr-3.4Si) cast relative to Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast
standard
Kennametal Stellite Tribaloy T-400 datasheet
heat treatment
as-cast
Tribaloy T-800 (Co-28Mo-17Cr-3.4Si) cast
standard
Kennametal Stellite Tribaloy T-800 datasheet
heat treatment
as-cast