Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Cobalt Alloy/Stellite 21 (Co-28Cr-5Mo-2.5Ni) cast vs Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast

Stellite 21 (Co-28Cr-5Mo-2.5Ni) cast vs Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast

Property comparison of Stellite 21 (Co-28Cr-5Mo-2.5Ni) cast and Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast, both cobalt alloy.

Cobalt Alloy3 compared properties
PropertyStellite 21 (Co-28Cr-5Mo-2.5Ni) castTribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) castDifference
Density8,330 kg/m³8,900 kg/m³+7%
Brinell hardness33 HB55 HB+67%
Melting point1,365 °C1,314 °C-4%

Difference is Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast relative to Stellite 21 (Co-28Cr-5Mo-2.5Ni) cast. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Stellite 21 (Co-28Cr-5Mo-2.5Ni) cast
grade
R30021
standard
Kennametal Stellite datasheet (Stellite 21 Alloy Technical Data)
heat treatment
as-cast
Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast
grade
standard
Kennametal Stellite Tribaloy T-400 datasheet
heat treatment
as-cast

What else is in Engineering Database

Related comparisons

View each material