Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Cobalt Alloy/Stellite 6B (Co-28Cr-4W-1C) wrought vs Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast

Stellite 6B (Co-28Cr-4W-1C) wrought vs Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast

Property comparison of Stellite 6B (Co-28Cr-4W-1C) wrought and Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast, both cobalt alloy.

Cobalt Alloy3 compared properties
PropertyStellite 6B (Co-28Cr-4W-1C) wroughtTribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) castDifference
Density8,390 kg/m³8,900 kg/m³+6%
Brinell hardness36 HB55 HB+53%
Melting point1,310 °C1,314 °C0%

Difference is Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast relative to Stellite 6B (Co-28Cr-4W-1C) wrought. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Stellite 6B (Co-28Cr-4W-1C) wrought
grade
R30016
standard
Kennametal Stellite / High Temp Metals (Stellite 6B Technical Data)
heat treatment
solution heat-treated
Tribaloy T-400 (Co-28Mo-8.5Cr-2.5Si) cast
grade
standard
Kennametal Stellite Tribaloy T-400 datasheet
heat treatment
as-cast

What else is in Engineering Database

Related comparisons

View each material