| Property | Ti-6Al-6V-2Sn Sheet/Strip/Plate Annealed | Ti-6Al-6V-2Sn Solution Treated and Aged | Difference |
|---|---|---|---|
| Yield strength | 965.3 MPa | 1,103 MPa | +14% |
| Tensile strength | 1,034 MPa | 1,207 MPa | +17% |
| Elongation | 10 % | 8 % | -20% |
| Elastic modulus | 110,316 MPa | 110,300 MPa | 0% |
| Shear modulus | 42,748 MPa | 42,700 MPa | 0% |
| Poisson ratio | 0.31 | 0.31 | 0% |
| Density | 4,540 kg/m³ | 4,539 kg/m³ | 0% |
Difference is Ti-6Al-6V-2Sn Solution Treated and Aged relative to Ti-6Al-6V-2Sn Sheet/Strip/Plate Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-6Al-6V-2Sn
- standard
- MIL-HDBK-5J
- heat treatment
- Annealed
- grade
- Ti-6Al-6V-2Sn
- standard
- AMS 4971 / AMS 4979
- heat treatment
- Solution Treated and Aged
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators