Ti-6Al-6V-2Sn Solution Treated and Aged vs Ti-6Al-7Nb (TIMETAL 367) Annealed
Property comparison of Ti-6Al-6V-2Sn Solution Treated and Aged and Ti-6Al-7Nb (TIMETAL 367) Annealed, both titanium alloy.
| Property | Ti-6Al-6V-2Sn Solution Treated and Aged | Ti-6Al-7Nb (TIMETAL 367) Annealed | Difference |
|---|---|---|---|
| Yield strength | 1,103 MPa | 900 MPa | -18% |
| Tensile strength | 1,207 MPa | 1,000 MPa | -17% |
| Elongation | 8 % | 12 % | +50% |
| Elastic modulus | 110,300 MPa | 112,500 MPa | +2% |
| Density | 4,539 kg/m³ | 4,520 kg/m³ | 0% |
| Melting point | 1,660 °C | 1,015 °C | -39% |
Difference is Ti-6Al-7Nb (TIMETAL 367) Annealed relative to Ti-6Al-6V-2Sn Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-6Al-6V-2Sn
- standard
- AMS 4971 / AMS 4979
- heat treatment
- Solution Treated and Aged
- grade
- Ti-6Al-7Nb
- standard
- ISO 5832-11 / ASTM F1295
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators