Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed vs Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged
Property comparison of Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed and Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged, both titanium alloy.
| Property | Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed | Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged | Difference |
|---|---|---|---|
| Yield strength | 966 MPa | 1,103 MPa | +14% |
| Tensile strength | 1,035 MPa | 1,172 MPa | +13% |
| Elongation | 15 % | 10 % | -33% |
| Elastic modulus | 114,000 MPa | 114,000 MPa | 0% |
| Density | 4,540 kg/m³ | 4,640 kg/m³ | +2% |
| Reduction in area | 30 % | 20 % | -33% |
Difference is Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged relative to Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-6Al-2Sn-4Zr-2Mo-0.1Si
- standard
- AMS 4976
- heat treatment
- Annealed (1800°F)
- grade
- Ti-6Al-2Sn-4Zr-6Mo
- standard
- Mil-T-9047 / AMS 4981
- heat treatment
- Solution Treated and Aged
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators