Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged vs Ti-6Al-6V-2Sn Annealed
Property comparison of Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged and Ti-6Al-6V-2Sn Annealed, both titanium alloy.
| Property | Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged | Ti-6Al-6V-2Sn Annealed | Difference |
|---|---|---|---|
| Yield strength | 1,103 MPa | 965 MPa | -13% |
| Tensile strength | 1,172 MPa | 1,034 MPa | -12% |
| Elongation | 10 % | 10 % | 0% |
| Elastic modulus | 114,000 MPa | 110,300 MPa | -3% |
| Density | 4,640 kg/m³ | 4,539 kg/m³ | -2% |
| Melting point | 1,635 °C | 1,660 °C | +2% |
Difference is Ti-6Al-6V-2Sn Annealed relative to Ti-6Al-2Sn-4Zr-6Mo (TIMETAL 6246) Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-6Al-2Sn-4Zr-6Mo
- standard
- Mil-T-9047 / AMS 4981
- heat treatment
- Solution Treated and Aged
- grade
- Ti-6Al-6V-2Sn
- standard
- AMS 4978 / AMS 4918
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators