Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Titanium Alloy/Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed vs Ti-6Al-2Sn-4Zr-2Mo Forging STA (Duplex Annealed)

Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed vs Ti-6Al-2Sn-4Zr-2Mo Forging STA (Duplex Annealed)

Property comparison of Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed and Ti-6Al-2Sn-4Zr-2Mo Forging STA (Duplex Annealed), both titanium alloy.

Titanium Alloy5 compared properties
PropertyTi-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) AnnealedTi-6Al-2Sn-4Zr-2Mo Forging STA (Duplex Annealed)Difference
Yield strength966 MPa827.4 MPa-14%
Tensile strength1,035 MPa896.3 MPa-13%
Elongation15 %10 %-33%
Elastic modulus114,000 MPa113,764 MPa0%
Density4,540 kg/m³4,540 kg/m³0%

Difference is Ti-6Al-2Sn-4Zr-2Mo Forging STA (Duplex Annealed) relative to Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Ti-6Al-2Sn-4Zr-2Mo-0.1Si (ATI 6-2-4-2Si) Annealed
grade
Ti-6Al-2Sn-4Zr-2Mo-0.1Si
standard
AMS 4976
heat treatment
Annealed (1800°F)
Ti-6Al-2Sn-4Zr-2Mo Forging STA (Duplex Annealed)
grade
Ti-6Al-2Sn-4Zr-2Mo
standard
MIL-HDBK-5J
heat treatment
Solution Treated and Aged (Duplex Annealed)

What else is in Engineering Database

Related comparisons

View each material