Carbon Steel12 compared properties
PropertySteel 12MCh GOST 20072-74Steel 13Ch14N3V2FR GOST 5949-75Difference
Yield strength235 MPa735 MPa+213%
Tensile strength410 MPa930 MPa+127%
Elongation21 %14 %-33%
Elastic modulus212,000 MPa200,000 MPa-6%
Shear modulus82,000 MPa77,000 MPa-6%
Poisson ratio0.290.3+3%
Density7,850 kg/m³7,850 kg/m³0%
Brinell hardness217 HB302 HB+39%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel 13Ch14N3V2FR GOST 5949-75 relative to Steel 12MCh GOST 20072-74. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel 12MCh GOST 20072-74
standard
GOST
Steel 13Ch14N3V2FR GOST 5949-75
standard
GOST

What else is in Engineering Database

Related comparisons

View each material