PropertyNylon 6 (PA6) UnfilledPA11 (Polyamide 11 Rilsan)Difference
Tensile strength80 MPa48 MPa-40%
Elongation30 %280 %+833%
Poisson ratio0.40.40%
Density1,130 kg/m³1,030 kg/m³-9%
Thermal conductivity0.25 W/m·K0.23 W/m·K-8%
Specific heat1,700 J/kg·K1,600 J/kg·K-6%
Coefficient of thermal expansion0.00008 1/K0.00011 1/K+37%

Difference is PA11 (Polyamide 11 Rilsan) relative to Nylon 6 (PA6) Unfilled. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Nylon 6 (PA6) Unfilled
standard
ASTM
PA11 (Polyamide 11 Rilsan)
standard
ASTM

What else is in Engineering Database

Related comparisons

View each material