Polymer7 compared properties
PropertyFEP (Fluorinated Ethylene Propylene Teflon FEP)Nylon 6 (PA6) UnfilledDifference
Tensile strength20 MPa80 MPa+300%
Elongation300 %30 %-90%
Poisson ratio0.480.4-17%
Density2,150 kg/m³1,130 kg/m³-47%
Thermal conductivity0.25 W/m·K0.25 W/m·K0%
Specific heat1,050 J/kg·K1,700 J/kg·K+62%
Coefficient of thermal expansion0.000135 1/K0.00008 1/K-41%

Difference is Nylon 6 (PA6) Unfilled relative to FEP (Fluorinated Ethylene Propylene Teflon FEP). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

FEP (Fluorinated Ethylene Propylene Teflon FEP)
standard
ASTM
Nylon 6 (PA6) Unfilled
standard
ASTM