NF 16MC5 vs NF 25CD4
Property comparison of NF 16MC5 and NF 25CD4, both carbon steel.
| Property | NF 16MC5 | NF 25CD4 | Difference |
|---|---|---|---|
| Yield strength | 700 MPa | 600 MPa | -14% |
| Tensile strength | 980 MPa | 780 MPa | -20% |
| Elongation | 9 % | 14 % | +56% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 456 J/kg·K | 458 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is NF 25CD4 relative to NF 16MC5. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
NF 16MC5
- standard
- NF
- heat treatment
- case-hardened
NF 25CD4
- standard
- NF
- heat treatment
- —
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators