PropertyNF 16NC6NF 25CD4Difference
Yield strength800 MPa600 MPa-25%
Tensile strength1,100 MPa780 MPa-29%
Elongation9 %14 %+56%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat456 J/kg·K458 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is NF 25CD4 relative to NF 16NC6. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NF 16NC6
standard
NF
heat treatment
case-hardened
NF 25CD4
standard
NF
heat treatment

What else is in Engineering Database

Related comparisons

View each material