Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/NF 16MC5 vs NF 20MC5

NF 16MC5 vs NF 20MC5

Property comparison of NF 16MC5 and NF 20MC5, both carbon steel.

Carbon Steel11 compared properties
PropertyNF 16MC5NF 20MC5Difference
Yield strength700 MPa850 MPa+21%
Tensile strength980 MPa1,200 MPa+22%
Elongation9 %7 %-22%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat456 J/kg·K457 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is NF 20MC5 relative to NF 16MC5. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NF 16MC5
standard
NF
heat treatment
case-hardened
NF 20MC5
standard
NF
heat treatment
case-hardened