Castable Refractory (Dense 60% Al2O3) vs Molybdenum (Mo pure >99.94%)
Property comparison of Castable Refractory (Dense 60% Al2O3) and Molybdenum (Mo pure >99.94%), both refractory.
| Property | Castable Refractory (Dense 60% Al2O3) | Molybdenum (Mo pure >99.94%) | Difference |
|---|---|---|---|
| Density | 2,500 kg/m³ | 10,220 kg/m³ | +309% |
| Thermal conductivity | 1.2 W/m·K | 138 W/m·K | +11400% |
| Coefficient of thermal expansion | 0.000007 1/K | 0.000005 1/K | -27% |
Difference is Molybdenum (Mo pure >99.94%) relative to Castable Refractory (Dense 60% Al2O3). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- cast_cured
- grade
- —
- heat treatment
- —
- standard
- ASTM
- grade
- Mo pure
- heat treatment
- Stress-Relieved
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators