Leaded Muntz metal C36500 vs Special Alloy C99300

Property comparison of Leaded Muntz metal C36500 and Special Alloy C99300, both aluminum alloy.

Aluminum Alloy11 compared properties
PropertyLeaded Muntz metal C36500Special Alloy C99300Difference
Yield strength138 MPa379 MPa+175%
Tensile strength372 MPa655 MPa+76%
Elongation45 %2 %-96%
Elastic modulus105,000 MPa100,000 MPa-5%
Shear modulus40,000 MPa37,000 MPa-8%
Poisson ratio0.320.34+6%
Density8,800 kg/m³8,500 kg/m³-3%
Thermal conductivity155 W/m·K155 W/m·K0%
Specific heat900 J/kg·K900 J/kg·K0%
Coefficient of thermal expansion0.000023 1/K0.000023 1/K0%
Melting point580 °C580 °C0%

Difference is Special Alloy C99300 relative to Leaded Muntz metal C36500. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Leaded Muntz metal C36500
standard
ANSI
heat treatment
As hot rolled
Special Alloy C99300
standard
ANSI
heat treatment

What else is in Engineering Database

Related comparisons

View each material