CSN 424415 vs Leaded Muntz metal C36500
Property comparison of CSN 424415 and Leaded Muntz metal C36500, both aluminum alloy.
| Property | CSN 424415 | Leaded Muntz metal C36500 | Difference |
|---|---|---|---|
| Yield strength | 110 MPa | 138 MPa | +25% |
| Tensile strength | 200 MPa | 372 MPa | +86% |
| Elastic modulus | 73,000 MPa | 105,000 MPa | +44% |
| Shear modulus | 26,000 MPa | 40,000 MPa | +54% |
| Poisson ratio | 0.33 | 0.32 | -3% |
| Density | 2,700 kg/m³ | 8,800 kg/m³ | +226% |
| Thermal conductivity | 155 W/m·K | 155 W/m·K | 0% |
| Specific heat | 900 J/kg·K | 900 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000023 1/K | 0.000023 1/K | 0% |
| Melting point | 580 °C | 580 °C | 0% |
Difference is Leaded Muntz metal C36500 relative to CSN 424415. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
CSN 424415
- standard
- CSN
- heat treatment
- —
Leaded Muntz metal C36500
- standard
- ANSI
- heat treatment
- As hot rolled
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators